Typical shrinkage 10-11% at 325°F/1hr.
High-tenacity polyester yarn is twisted into a smooth, round, 3-ply construction. It provides improved heat range, added strength and excellent heat shrink characteristics. Increased yield over braided constructions makes it the most economical for high-volume automatic applications. Available on a straight tube or cone-wound.
Suggested Coatings:
“CL” Polyurethane, “W” Wax, “X” Untreated.
Part Number | Approx. Diameter Inches | Nominal Break Lbs. | Yield Yds./Lbs. Uncoated | Standard Put-Up |
DRT-20 | .012 | 16 | 3260 | 1 lb. |
DRT-30 | .016 | 35 | 1719 | 1, 2 lbs. |
DRT-45 | .026 | 45 | 1441 | 1, 2, 4, 6 lbs. |
DRT-50 | .028 | 50 | 1190 | 1, 2, 4, 6 lbs. |
DRT-65 | .030 | 65 | 1060 | 1, 2, 4, 6 lbs. |
DRT-100 | .040 | 85 | 860 | 1, 2, 4, 6 lbs. |